添加CeO2的二硅酸锂微晶玻璃的力学改性研究Investigation of Improving Mechanical Properties of Lithium Disilicate Glass-Ceramics by CeO2 Addition
周丽敏,姬玉,周毅
摘要(Abstract):
当前二硅酸锂微晶玻璃在牙科领域的应用仍存在脆性大、强度低的问题,因此本研究采用熔融快冷法制备了不同CeO_2添加量(0-3 mol%)的Li_2O-SiO_2系玻璃,并在700℃和800℃下结晶热处理得到Li_2Si_2O_5系微晶玻璃,系统研究了CeO_2添加对材料力学改性的影响。结果表明,适量CeO_2添加(2 mol%)能显著优化微晶玻璃的力学性能。800℃晶化时,该体系微晶玻璃的力学性能得到有效改善:维氏硬度可达7.33 GPa、断裂韧性达到2.95 MPa·m~(1/2)和抗弯强度达到189.65 MPa。添加过量CeO_2(3 mol%)会导致主晶相转变为α-石英与锂辉石,引起力学性能下降。CeO_2添加量为2 mol%,晶化温度为800℃,是该材料体系的最佳工艺条件。本研究为Li_2Si_2O_5系微晶玻璃在牙科修复领域的进一步应用提供了理论依据。
关键词(KeyWords): 二硅酸锂微晶玻璃;CeO_2添加;晶化温度;力学性能;增韧机制
基金项目(Foundation): 国家自然科学基金(51902221)
作者(Author): 周丽敏,姬玉,周毅
DOI: 10.16666/j.cnki.issn1004-6178.2026.04.012
参考文献(References):
- [1] AL-JOHANI H, HAIDER J, SATTERTHWAITE J, SILIKAS N. Lithium Silicate-Based Glass Ceramics in Dentistry:A Narrative Review[J]. Prosthesis, 2024, 6(3):478-505.
- [2] PHARK J H, DUARTE JR S. Microstructural considerations for novel lithium disilicate glass ceramics:A review[J]. Journal of Esthetic and Restorative Dentistry, 2022, 34(1):92-103.
- [3] HALLMANN L, ULMER P, KERN M. Effect of microstructure on the mechanical properties of lithium disilicate glass-ceramics[J]. Journal of the Mechanical Behavior of Biomedical Materials, 2018, 82:355-370.
- [4] HOLAND W, RHEINBERGER V, APEL E, VAN T HOEN C, HOLAND M, DOMMANN A, OBRECHT M, MAUTH C, GRAFHAUSNER U. Clinical applications of glass-ceramics in dentistry[J]. Journal of Materials Science:Materials in Medicine, 2006, 17(11):1037-1042.
- [5] VALLERINI B F, SILVA L D, VILLAS-B??AS M O C, PEITL O, ZANOTTO E D. Microstructure and mechanical properties of an experimental lithium disilicate dental glass-ceramic[J]. Ceramics International, 2024, 50(1 Part A):188-196.
- [6] MARZOUK M A, ELBATAL H A, ELBATAL F H, AZOOZ M A. Preparation and Characterization of Nano Glass-ceramics from CeO2-doped Li2O-SiO2 System for Dental Applications[J]. Silicon, 2024, 16(2):457-468.
- [7] ALVES M F R P, BAPTISTA I O, GADDAM A, FERREIRA S, FERNANDES M H F. Influence of ZnO and CeO2 addition on the structure, properties and antibacterial activity of lithium silicate–based glass-ceramics[J]. Journal of Alloys and Compounds, 2026:186971.
- [8] LI S, WEI C, WANG W, WANG P, LIU Y. Fracture toughness and R-curve behavior of laminated ZrB2-SiC/SiCw ceramic[J]. Journal of Alloys and Compounds, 2019, 784:96-101.
- [9] WEI C, LIU Z, WU Y, LIU Y, ZHANG H, WANG P, SUN Q, ZHOU L. Toughness and R-curve behaviour of laminated Si3N4/SiCw ceramics[J]. Ceramics International, 2021, 47:18693-18698.
- [10] VILCHEZ V, PELISSARI P I B G B, PANDOLFELLI V C, BOUVILLE F. Mixed-mode fracture model to quantify local toughness in nacrelike alumina[J]. Journal of the European Ceramic Society, 2023, 43:4472-4481.
- [11] LIEN W, ROBERTS H W, PLATT J A, VANDEWALLE K S, HILL T J. Microstructural evolution and physical behavior of a lithium disilicate glassceramic[J]. Dental Materials, 2015, 31(8):928-940.
- [12] ANSTIS G R, CHANTIKUL P, LAWN B R, MARSHALL D B. A critical evaluation of indentation techniques for measuring fracture toughness:I, direct crack measurements[J]. Journal of the American Ceramic Society, 1981, 64(9):533-538.
- [13] RAMACHANDRAN N, SHETTY D K. Rising Crack-Growth-Resistance(R-Curve)Behavior of Toughened Alumina and Silicon Nitride[J]. Journal of the American Ceramic Society, 1991, 74(10):2634-2641.
- [14] KRAIPOK A, MAMANEE T, RUANGSURIYA J, LEENAKUL W. Investigation of phase formation and mechanical properties of lithium disilicate glass-ceramic doped CeO2[J]. Journal of Non-Crystalline Solids, 2021, 564:120772.
- [15] XUE W J, XIE Z P, LIU G W, LIU W, YI J. R-curve behavior of 3Y-TZP at cryogenic temperatures[J]. Journal of the American Ceramic Society, 2011, 94(9):2775-2778.
- [16] LEI Y, HE Y, CHEN F F, XU J. Effect of Mineralizers and Reaction Conditions on the Formation of Cristobalite[J]. InterCeram:International Ceramic Review, 2015, 64(4):214-218.
- [17] HU A M, LIANG K M, ZHOU F, WANG G L, PENG F. Phase transformations of Li2O–Al2O3–SiO2 glasses with CeO2 addition[J]. Ceramics International, 2005, 31(1):11-14.
- [18] GUAN B, LIU S, LIU J, ZHENG X, SHAN X, JI Y, QIN Z, ZHU J, ZHENG Q, WANG L, MAURO J C, DING L. Phase evolution and mechanical properties in Li2O–Al2O3–SiO2 glass-ceramics:Influence of heat treatment parameters[J]. Journal of the American Ceramic Society, 2025, 109:e70364.
- [19] UMARI P, PASQUARELLO A, DAL CORSO A. Raman scattering intensities in α-quartz:A first-principles investigation[J]. Physical Review B, 2001, 63(9):094305.
- [20] HOU G, ZHANG C, FU W, LI G, XIA J, PING Y. Improvement of mechanical strength in Y3+/La3+co-doped silicate glasses for display screen[J]. Ceramics International, 2019, 45(9):11850-11855.